[TheForge] 72 inch belts

Peter Fels And Phoebe Palmer artgawk at thegrid.net
Thu Jun 28 04:26:01 EDT 2007


Doncha think you are being a bit abrasive there Frosty?

I like
> http://www.acutabove.com/

Pete

Jerry Frost wrote:
> 
> From: "Daniel Kretchmar" <dan at irontreeworks.com>
> 
> 
> 
>>
>> Anyone want to recommend a good source for 72 inch belts?  Also, what 
>> grits do you recommend?
>>
>> Dan
>> www.irontreeworks.com
>>
> 
> 
> And I thought it was bad when my 36" belt started getting tight!
> 
> I'd recommend laying off the grits.
> 
> <grin>
> 
> Frosty
> -------------------------------
> If it ain't forged
> it ain't real.
> Wrought iron is.
> The FrostWorks
> 
> Meadow Lakes, AK.
> 
> http://www.artmetalradio.com/
> 
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 
> 


More information about the TheForge mailing list