[TheForge] oxy-propylene/Henrob
Kathy
keporter at comcast.net
Fri Jun 22 17:28:09 EDT 2007
Clyde,
The Henrob does work with oxy-propane, but no claims to superior cutting or
welding characteristics are claimed for this torch with any fuel but acetylene.
So, why would you put up with its disadvantages, without any hoped for
advantages?
Mikey
-----Original Message-----
From: theforge-bounces at mailman.qth.net [mailto:theforge-bounces at mailman.qth.net]
On Behalf Of Peter Fels And Phoebe Palmer
Sent: Friday, June 22, 2007 12:39 AM
To: clyde at fibernetcc.com; Sponsored by ABANA
Subject: Re: [TheForge] oxy-propylene/Henrob
Hi Clyde;
I ditched the clunky aluminum handle and the cutting tube on my
Henrob and liked it a lot better...then somebody walked into the
shop, cut the hoses and stole it off the wall...goofy! They
couldn't have known what it was.
I'm presently dinking away at cutting another one down even
further..it has a lot of excess weight still.
Clyde Wynia wrote:
> I'd love a copy. Thanks. And BTW, I have a Henrob and always thought it was
> for oxy/acetylene only, not propane. Do they work with propane? If so do you
> need different tips?
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Ron Childers
> Sent: Thursday, June 21, 2007 7:46 AM
> To: 'Sponsored by ABANA'
> Subject: RE: [TheForge] oxy-propylene
>
> It's a mind set; I welded with propane in a Henrob torch and it worked fine.
>
>
> Btw, if anyone needs a copy of the Henrob manual let me know and I'll e-mail
> it as an attachment.
>
> Ron C
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Larry Ruebush
> Sent: Thursday, June 21, 2007 8:24 AM
> To: Sponsored by ABANA
> Subject: Re: [TheForge] oxy-propylene
>
> I have welded with a propane/ox torch for over 40 years.
> Don't know why some people say it can't be done
> Larry Ruebush
> west central IL
> ----- Original Message -----
> From: "Bruce Freeman" <FREEMAB at pt.fdah.com>
> To: <theforge at mailman.qth.net>
> Sent: Thursday, June 21, 2007 7:02 AM
> Subject: RE: [TheForge] oxy-propylene
>
>
> I have no experience with this, but previous discussions on this forum
> concluded it was impossible to weld with propane.
>
> But cutting is done with the oxygen after heading the steel. What
> difference would the propane make to that?
>
> Bruce
> NJ
>
>>>> gblacksmith at alamedanet.net 6/20/2007 9:53 PM >>>
> Oxy-Propane? It is cheaper for the propane, but more difficult to cut and
> weld with. I have not used it, so I can't speak from experience.
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net]On Behalf Of Chris Caswell
> Sent: Wednesday, June 20, 2007 5:24 PM
> To: Forge
> Subject: [TheForge] oxy-propylene
>
>
> Greetings all
>
> I am considering switching to oxy-propylene (supposedly is cheaper and
> will last longer) - I use the torches for cutting and spot heating only.
> Any opinions?
>
> Chris Caswell
> Caswell Wood & Iron
> Burlington, VT
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
> No virus found in this incoming message.
> Checked by AVG Free Edition.
> Version: 7.5.472 / Virus Database: 269.9.1/857 - Release Date: 6/20/2007
> 2:18 PM
>
> No virus found in this outgoing message.
> Checked by AVG Free Edition.
> Version: 7.5.472 / Virus Database: 269.9.1/857 - Release Date: 6/20/2007
> 2:18 PM
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge