[TheForge] oxy-propylene
Grant Marcoux
gblacksmith at alamedanet.net
Wed Jun 20 21:53:38 EDT 2007
Oxy-Propane? It is cheaper for the propane, but more difficult to cut and
weld with. I have not used it, so I can't speak from experience.
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net]On Behalf Of Chris Caswell
Sent: Wednesday, June 20, 2007 5:24 PM
To: Forge
Subject: [TheForge] oxy-propylene
Greetings all
I am considering switching to oxy-propylene (supposedly is cheaper and
will last longer) - I use the torches for cutting and spot heating only.
Any opinions?
Chris Caswell
Caswell Wood & Iron
Burlington, VT
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
No virus found in this incoming message.
Checked by AVG Free Edition.
Version: 7.5.472 / Virus Database: 269.9.1/857 - Release Date: 6/20/2007
2:18 PM
No virus found in this outgoing message.
Checked by AVG Free Edition.
Version: 7.5.472 / Virus Database: 269.9.1/857 - Release Date: 6/20/2007
2:18 PM
More information about the TheForge
mailing list