When I was in welding school we were taught that 7018 sounded like frying bacon
if the cable polarity was correct. After becoming used to the sounds of 7018 on
correct polarity versus wrong polarity, I noted the sound as barely reminiscent
of frying bacon. Probably all such advice has some value in retrospect, but not
as a guide during the learning curve. This kind of advice is given by writers
and instructors who are parroting instructions written half a century before, to
students with a different mind set, who could be easily coerced into nodding
their assent (shutting their yaps) and privately doing their best to conform.
This isn't WW2, and today's welding students are very different; welding advice
should be updated to suit the time and place.
Mikey
-----Original Message-----
From: theforge-bounces at mailman.qth.net [mailto:theforge-bounces at mailman.qth.net]
On Behalf Of Jerry Frost
Sent: Friday, June 01, 2007 12:57 PM
To: Sponsored by ABANA
Subject: Re: [TheForge] Stick welding
There've been a lot of good tips so far and listening
to the arc is high on the list. The sound will depend
on what you're doing though. DC should sound more like
an air escaping hiss than frying bacon. AC should sound
like gently frying bacon. Crackling in any case isn't
good.
While you're practicing with pencil/pen and paper hold
it with a pair of pliers for the full effect.
Frosty
-------------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks
Meadow Lakes, AK.
http://www.artmetalradio.com/
From: "Jeffrey Polaski" <jeff.polaski at rgs.uci.edu>
Here are a couple of tips I picked up in welding
class...
First, pay attention to the *sound* while you are
welding... It's hard
to describe over email, but you want to get a sound
like bacon frying.
Second, practice making the correct hand motions with a
pen and paper.
The idea is to train your hand to make the right
motions. If you are
using a crescent shape, just fill up a page or two with
that shape using
a pen and paper. Lock your wrist and try to hold the
pen like you would
an electrode. After doing that, switch to using the
electrode without
any power. Just make the motions to get familiar with
the feel of it.
The book "Modern Welding" does a good job explaining
this
Third, try welding to failure... Be prepared to
sacrifice some scrap and
dial it up a few notches *higher* than you should. See
what happens when
you weld *through* your practice piece. It will give
you a much better
idea of what the settings should be.
I don't weld much, but those tips helped out in class.
Jeff Polaski
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list