Hey Andy,
Good point, I was scrounging for something for a burner bracket and
found just the right size in a galvanized pipe. Tried burning the
galvanizing off of it and having had fume fever before it just scared
the hell out of me. Scrapped it. Going for store bought black iron.
Harry
Andy Gladish wrote:
> I would want to make sure that the vessel I use for a forge shell is not
> galvanized, IE zinc coated.
> Believe all the well tanks are- the fumes are awful when they get hot.
>