[TheForge] where do I get?

Peter Fels And Phoebe Palmer artgawk at thegrid.net
Mon Jul 30 04:17:51 EDT 2007


Touchmarks
Dave;
I think Grant Sarver still makes them...he's the Offcenter Forge 
guy that makes the nifty tongs and stuff.

Cutting Galvanized tanks
Jerry;
I wouldn't be bold enough to disagree with you normally....but..
Having had metal fume fever ( ZINC SHAKES) from zinc fumes ,3 
times worth mentioning...my opinion differs.
Most evident was the projectile vomiting and crapping...really 
projectile and very vivid. The gut squeezes shut in the middle 
somewhere and a violent spastic waves travel both directions at 
once. Then there's the chills which take over your sensory world.
It was comparable to heavy chemotherapy.
I could go on but..that gives you a hint, except to note it seems 
to be cumulative to a considerable extent.
A good particle filter will take out a fair part of the nasty 
stuff. Muriatic acid will remove it pretty well...pf

Dave Mudge wrote:
> Good Morning Group,
> Can you recommend a manufacturer of touch mark stamps?
> Bought my original about 20 years ago but don't remember where.
> thanks,
> dave mudge
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 
> 


More information about the TheForge mailing list