From: "Peter Fels And Phoebe Palmer"
<artgawk at thegrid.net>
> aww Mikey; Guess i'll cancel my plans to picket in
> front of your shop then.
>
Geeze Pete. Does that mean you're not picking me up on
the way? I had my sign made and everything. Oh well I
guess I'll drink the beer I had packed. <sigh>
> The reason i brought it up is that, prior to your
> excellent book, many naturally aspirated forges have
> had difficulty making a high welding heat. Many
> smiths have gone for blown forges for that reason.
> I've read recommendations that owners of cool forges
> ( hey, cool forge dude) carefully polish the inside
> of their burners, fool with venturi placement and so
> on, all to gain some bit more flow.
> So it always seemed to me that facing up from below
> would be a bit more efficient...one can always choke
> it down if it's too much.
> In a related consideration, many forges pull the
> exhaust off the top, where the hottest gases hang
> out, spewing extra BTUs
>
I don't know how many decades commercial forge builders
used really poor linear inducers for their burners.
Most wouldn't reach welding heat at all unless you used
a really agressive flux. The result being the myth that
a naturally aspirated burner couldn't reach welding
heat. I wouldn't go so far as to say it lead to selling
more expensive gun burner forges but . . .
Anyway, the truth is a burner is nothing more than a
system for introducing a flamable material and air in a
metered ratio, mixing them and delivering them to the
desired location. Both gun (blown) and naturally
aspirated burners deliver air under pressure, that
result is the same either way. A gun has the advantage
of delivering it in a more robust manner and is less
sensitive to outside conditions like open or closed
forge doors, etc. A naturally aspirated burner will
usually need to be adjusted for changing conditions of
smaller degree.
In either case the effects of natural convection are so
slight as to be a zero effect variable. This isn't
necessarily true with the commercially produced forge
burners as most are made to barely do the job. They
simply do not have any reserve to overcome any level of
adverse conditions. In this case convection may indeed
effect performance to a noticeable extent.
>
>
> The test, while very interesting, isn't all that
> relevant because you don't have 2000* of hot gas
> pushing up from below.
>
Actually that test illustrates the only effect
convection has in a forge. The burner is introducing
air and fuel into the forge chamber under pressure,
combustion causes them to expand but they're already
moving in one direction; towards the exhaust port
whether that is a dedicated port as in a melting
furnace or an open door like most forges. Force seeks
the route of least resistance; Always.
>> 2. "The greater heat of the top of the forge would
>> cook the burner faster."
>>
>> The minuet the burner is shut down, interior gases
>> can enter the burner through
>> buoyancy; this is called the "chimney effect," and
>> is prevented by closing the
>> burner's choke completely during shutdown. While
>> running, the burner prevents
>> the forge gases from entering. Refrigeration effect
>> from the expanding fuel gas
>> is sufficient to keep the burner from overheating do
>> to conduction and
>> convection gain from the forge body and nearby
>> exhaust gas. These rules apply
>> equally to top mounted burners (the overwhelmingly
>> dominant mounting choice),
>> whether they are placed at vertical down (90°) for
>> spot heating, or 3” down from
>> top dead center (on a 14" diameter forge) to create
>> a swirl.
>>
As Mike says so well, the only time convection is a
problem for a downward aiming burner is on shut down
when gasses super heated in the forge will rise through
the burner. This can burn up your gas hose but is
unlikely to actually damage the burner itself. Shutting
the choke completely or just stuffing a piece of
Kaowool (or whatever) into the intake eliminates this
potential problem.
>>
>> Finally, why is vertical down the dominate choice
>> even for swirl effect? Because
>> portable forges use ceramic fiber for most of the
>> interior insulation, and
>> placing a burner at the forge's top allows it to be
>> aimed directly at the
>> firebrick or kiln shelf slab on the forge's bottom.
>> Should you decide to use
>> Kastolite 3000 insulating refractory for the forge's
>> interior, instead of
>> insulating fiber and a kiln shelf floor, than the
>> burner placement can be
>> changed to whatever you find most convenient. Also,
>> solid refractory is a much
>> better choice for multiple use forge/furnaces, or
>> for a forge employed in billet
>> heating. A typical five gallon cylinder with a two
>> inch thick Kastolite 3000
>> refractory lining will still be portable
>> (approximately 65 lb.) On the other
>> hand the same forge built with ceramic fiber and a
>> kiln shelf floor can be
>> lifted comfortably with two fingers; it's all a
>> question of what features you
>> find most convenient.
>>
> Perhaps a burner target area of kastolite ( thanks
> for the reference) or kiln shelf would solve that.
> Speaking of that, i got an old carbide kiln shelf i
> cut up for a floor, very durable.
> Thanks Mikey...your answers are informed, considered
> and help a bunch!....pf
>
> Mikey
>
Careful consideration of the target material is
important and a small argument in favor of tangential
burner placement. A flame hitting something on a
tangent spreads the heat over a greater area so the
target material stays at a lower absolute temperature.