[TheForge] Burner angle conflagrations...
Peter Fels And Phoebe Palmer
artgawk at thegrid.net
Sat Jul 14 03:29:53 EDT 2007
Oy....disaster compounded by puns..a funny exposition Mikey!...pf
Kathy wrote:
> Actually, Frosty:
> Bad things happen to the crucible, after which, the melt pours out through the
> new hole, thus tending to make bad things happen to the burner...unless the
> furnace features an emergency drain hole; in which case, bad things happen to
> the floor (unless a sand filled emergency catch box was positioned below the
> furnace in advance); this is especially true if the floor is wooden.
>
> The sand box is, however, no guaranty of safety; if through inattention on the
> part of its attendant your cat is permitted to use it for a different kind of
> box, a smelly 'steam' explosion may ensue, reversing the molten stream's
> trajectory, possibly causing bodily injury. To add insult, severe nose clamping,
> accompanied by much public disapproval, may have to be endured in the hospital's
> emergency room.
>
> On the other hand, liquid metal flowing into the burner, and then catching the
> fuel hose on fire can also be exciting; either path tends toward much ringing of
> hands and "screaming like a girl," while the building goes up (and then falls
> down).
>
> Alas, fire departments never arrive in time to save the structure; only to
> prevent its being neatly consumed; provoking several trips to the dump. Thus
> you're at the dump while "in the dumps", so to speak, so at least your mood will
> be appropriate; that is, if you can get away from your insurance adjuster's
> awkward questions long enough to do anything constructive.
>
> Perhaps, the whole mess can be put down to high spirited frolicking around if
> you do all your casting on The Fourth; otherwise, I'm afraid the neighbors are
> bound to notice all such conflagrations. In any case, your wife is certain
> notice, necessitating the building of a dog house; fortunately a ready to hand
> site should have become available at this point, thus ending the whole incident
> on an upbeat note. I think that's very important, don't you? >:-)))
>
> Mikey
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net [mailto:theforge-bounces at mailman.qth.net]
> On Behalf Of Jerry Frost
> Sent: Friday, July 13, 2007 10:48 AM
> To: Sponsored by ABANA
> Subject: Re: [TheForge] Burner angle
>
> My pleasure Harry.
>
> If you want to use it as a melting furnace too, then
> you have to mount the burner(s) tangentially. The fire
> has to circulate around the crucible or bad things
> happen to the melt.
>
> Frosty
> -------------------------------
> If it ain't forged
> it ain't real.
> Wrought iron is.
> The FrostWorks
>
> Meadow Lakes, AK.
>
> http://www.artmetalradio.com/
>
> From: "Harry" <iowaharry at fastmail.net>
>
>
>> Thanks for the reply, Frosty,
>>
>> I had anticipated making a variety of forges. This
>> one may end up
>> doing double duty as melting pot as well. I
>> appreciate the info on
>> why one would choose direct or vortex. I have been
>> sitting on this
>> project for months. I have been dealing with a
>> rather aggressive
>> honey dew list. One item was erecting an above
>> ground pool. Now I
>> have someplace to run to when I get a burn. I'm
>> pretty sure SWMBO
>> won't cotton to me quenching anything in there, (at
>> least not while
>> she is looking <g>).
>>
>> Back to the shop, Harry
>>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list