I wouldn't think so. ITC 100 is a refractory coating, not just a
rigidizer. It greatly increases the efficiency of my forge. Less heat is
absorbed by the walls and is reflected back into the peice. My forge gets
heats up faster, gets hotter, and runs on less gas after I coat it with ITC
100.
Dan
----- Original Message -----
From: "Harry" <iowaharry at fastmail.net>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Friday, July 13, 2007 11:04 AM
Subject: [TheForge] ITC 100 or rigidizer
> Howdy all,
>
> My local kiln supply outfit does not carry ITC 100, is rigidizer an
> acceptable replacement? They said they had not heard of ITC 100 nor
> had anyone come in asking for it. I didn't get any further info on it
> as I just assumed I would order the ITC online.
>
> Thanks, Harry
> --
> Harry
> iowaharry at fastmail.net
>
> --
> http://www.fastmail.fm - A fast, anti-spam email service.
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list