[TheForge] Re: Making a drag bar
Jerry Frost
akfrosty at mtaonline.net
Thu Jul 12 14:31:40 EDT 2007
From: "Mike Spencer" <mspencer at tallships.ca>
>
> Jerry> ...an old truck spring for the actual drag
> bar.
>
> Frosty> No problem forging 5160 Jerry...
>
> I don't know about 5610 but I forged a replacement
> tine for my
> Troy-Built tiller from new truck spring -- offcut
> from the spring shop
> -- and it's on its 3rd year and doing fine.
>
> - Mike
>
> --
> Michael Spencer Nova Scotia, Canada
> .~.
>
> /V\
Yeah, that's the stuff; leaf spring is 5160. They all
are, as far as I know, since the mid 60's I think
anyway, but it maybe something different on heavy
trucks from the factory. How's that for unqualified
qualification? <grin>
The local spring shops all use 5160 for leaf springs of
whatever size and 9260 for coil springs. It's good
stuff, very forgiving within broad parameters.
Frosty
-------------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks
Meadow Lakes, AK.
http://www.artmetalradio.com/