Hi Phlip;
You can rip these out pretty quickly by using the old ring making
method of wrapping rod around a pipe and running down one side of
the coil with a torch or slitting disk. The trick is to pull as
you wrap.
To make the "D", simply cut off a strip down one side of the
pipe...that'll make cutting the coil easy.
Then a couple of swats to straighten and a quick zap with a
welder finishes them off....pete f
Dan Scheid wrote:
> Local Tack shop
> Dan Scheid
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Saint Phlip
> Sent: Tuesday, July 10, 2007 10:49 PM
> To: danqualman at mail.com; Sponsored by ABANA
> Subject: Re: [TheForge] D-rings
>
> Thanks, Dan, but these are a bit heavier than what I need. I'm looking
> for something that will secure the fabric walls of a tent I'm
> building. 9000 lb capacity is a bit...excessive.
>
> Gotta be someplace where I can buy a bundle of them for fairly light duty.
>
> On 7/11/07, Dan Brewer <danqualman at gmail.com> wrote:
> <http://www.northerntool.com/webapp/wcs/stores/servlet/NTESearch?storeId=697
> 0&N=0&Ntk=All&Ntt=d%20ring&Nty=1&D=d%20ring&Ntx=mode+matchallpartial&Dx=mode
>> +matchallpartial >
>>
>> http://wescoperformance.stores.yahoo.net/drings.html
>>
>> http://www.tandemloc.com/toc_tiedowns_other.asp
>>
>>
> <http://www.uscargocontrol.com/anchorpointsdrings-c-12.html?zenid=bc79d1a308
>> 2f9e099121be582345f887&gclid=CKjUmZHXno0CFQIPYwodmgXM6w>
>>
>> http://www.hoistquip.co.uk/documents/pdf/119.pdf
>>
>>
>>
>> -----Original Message-----
>> From: theforge-bounces at mailman.qth.net
>> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Saint Phlip
>> Sent: Tuesday, July 10, 2007 7:31 PM
>> To: Sponsored by ABANA
>> Subject: [TheForge] D-rings
>>
>> Anybody know where I can get a bunch of D-rings for a reasonable
>> price? I need about 50 of them, 1 1/4" bar, and I'd really rather not
>> have to forge them.
>>
>> Thanks,
>>
>> --
>> Saint Phlip
>>
>> Heat it up
>> Hit it hard
>> Repent as necessary.
>>
>> Priorities:
>>
>> It's the smith who makes the tools, not the tools which make the smith.
>>
>> Blessed be the self-righteous, for they shall inherit themselves.
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> password: anvil
>> ___________
>>
>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> password: anvil
>> ___________
>>
>>
>>
>
>
More information about the TheForge
mailing list