Chad, forge an old jack hammer bit
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Angels and Griffins
Armour Supply
Sent: Thursday, January 25, 2007 1:34 PM
To: theforge at mailman.qth.net
Subject: [TheForge] I am fireman and a blacksmith,In need of a good sorse
for HC or toolsteel in 1"
Good morning all this is my first post.
I am a fireman in northern Va and a black smith andI am hitting a
big snag in a very important and special project for work. about 10 ago the
only tool company worth a damn that did not use chince dutle iorn tool heads
went out of busness. Now the ony company making a 6' new your hook is using
ductle heads and the pry bar inds counldnt open a coke can. I have been
reclying 1045 crow bars to make new heads for my co workers, but i would
relay like to use 1095, L-6, or as seires steel but cant find any in 3/4" by
1 1/2" unless i buy multiple stock legnths from allmetal forge in Atlanta
wich i cant afford on the shops budget. doe any one have a sugestion for a
vender or alternative matrial. The tool head is used to breah 3/4" ply would
roofing, doors and just about anything you want to put a hole in. I would
love to make it durable enough to breech a block wall.
thanks
chad
_________________________________________________________________
Turn searches into helpful donations. Make your search count.
http://click4thecause.live.com/search/charity/default.aspx?source=hmemtaglin
e_donation&FORM=WLMTAG
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list