[TheForge] Kinyon Air Hammer Problem
Dan Tull
dantull at numail.org
Wed Jan 24 10:35:05 EST 2007
Went from 105psi to 85.
Hell, it's worth a try. What would it hurt?
----- Original Message -----
From: "Phil" <mobjak at yahoo.com>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Wednesday, January 24, 2007 8:03 AM
Subject: Re: [TheForge] Kinyon Air Hammer Problem
Dan:
What do you have your air pressure set on? This is a
different air scheme than the big blu.
This hammer has been running fine for the last 8 or so
years. It's just developed this problem in the last
week or so.
Thanks
Phil
--- Dan Tull <dantull at numail.org> wrote:
> My blu did that and Dean said to cut back on the air
> pressure , and it
> worked.
>
> ----- Original Message -----
> From: "Phil" <mobjak at yahoo.com>
> To: "Sponsored by ABANA" <theforge at mailman.qth.net>
> Sent: Tuesday, January 23, 2007 7:46 PM
> Subject: [TheForge] Kinyon Air Hammer Problem
>
>
> I'm trying to trouble shoot a problem with a kinyon
> style air hammer long distance, and I was hoping you
> all could help me out. This hammer is running the
> air
> scheme from the AFC web site. the guy that owns it
> says it goes up hard, and comes down soft. It goes
> up
> so hard that it broke the die spring on the cylinder
> rod.
>
> Can anyone suggest some probable causes of the
> problem?
>
> Thanks,
>
> Phil Rosche
> Summerville, SC
>
>
>
>
____________________________________________________________________________________
> Do you Yahoo!?
> Everyone is raving about the all-new Yahoo! Mail
> beta.
> http://new.mail.yahoo.com
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
____________________________________________________________________________________
Do you Yahoo!?
Everyone is raving about the all-new Yahoo! Mail beta.
http://new.mail.yahoo.com
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list