[TheForge] Shrinking Stainless Sheet metal

debmiller at fuse.net debmiller at fuse.net
Wed Jan 17 10:51:29 EST 2007


Hey Guys!
New question:
Who has process descriptions for heat shrinking stainless steel sheet metal after weld distortion. I am fairly familiar with the process for carbon steel, but stainless seems to be more of a mystery.  Or is it  better to do it with shrinking dies? I bet Reis has all the answers..............