[TheForge] help wanted ad
Wes Marquart
marquart at arlinn-tower.com
Wed Jan 10 00:30:09 EST 2007
All I can say is 'Here's another <American> job gone down the tubes'
Note where the Ref# is pointed at: " Backlog Elimination Center, Employment
and Training Administration, Division of Foreign Labor Certification"
Looks like we'll be seeing H1B's eliminating our positions next...
:{
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Kenneth Mayer
Sent: Tuesday, January 09, 2007 7:41 PM
To: theforge at mailman.qth.net
Subject: [TheForge] help wanted ad
This ad ran in Sunday's "The Record" newspaper in northern NJ.
www.northjersey.com afik the company makes ornamental ironwork, stairs and
fire escapes.
Ken
:-)
Company Information
Company Name: 37TH STREET IRON CO. INC.DEVINCENZO
Phone: 0513936780
Fax: (484) 270- 1600
Location: North Jersey Job Listings,US
Job Description
BLACKSMITH (Union City, NJ) Forges and repairs variety of metal articles,
such as tongs edged tools, hooks, chains, machines and structural
components, and agricultural implements as specified by work orders,
diagrams, or sample parts: Heats metal stock in blacksmiths forge or furnace
[Heater (forging)]. Hammers stock into specified size and shape on
blacksmiths anvil or positions stock on anvil of power hammer and depresses
pedal to hammer stock with varying force and rapidity. Forge-welds metal
parts by heating and hammering them together. Devises jigs and fixtures,
forges special hand tools, such as hammers or chisels and sets up for
blocks. Tempers or anneals forged articles [Heat Treater (heat treating)].
May record type of repair or fabrication of tools or machine components
performed during work shift to maintain daily activity report and records.
May cut, assemble and weld metal parts, using arc or acetylene welding
equipment [Welder, Combination (welding)]. May repair farm machinery and be
designated Blacksmith, Farm (agriculture). May be designated according to
articles forged as Special- Trackwork Blacksmith (r.r.trans.); Tool-Dresser
(forging). 40-hrs/wk. $400/wk. Exp: 2yrs. Send resume by fax to (484) 270-
1600 or by mail to Ref: No. P-05139-36780 KJo, Backlog Elimination Center,
Employment and Training Administration, Division of Foreign Labor
Certification, 1 Belmont Avenue, Suite 220, Bala Cynwyd, PA 19004.
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
--
No virus found in this incoming message.
Checked by AVG Free Edition.
Version: 7.5.432 / Virus Database: 268.16.7/620 - Release Date: 1/8/2007
4:12 PM
More information about the TheForge
mailing list