Well I shall add that to the sum of things I learnt today...thank you!
Rich M.
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Andrew Vida
> Sent: 07 January 2007 23:15
> To: Sponsored by ABANA
> Subject: Re: [TheForge] forged cross
>
>
>
>
> Rich Maynard wrote:
> > Umm, what's 'muck bar?'
>
> Unrefined wrought iron. It is very coarse and full of
> slag. It is
> considered the lowest grade.
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
> --
> No virus found in this incoming message.
> Checked by AVG Free Edition.
> Version: 7.5.432 / Virus Database: 268.16.7/619 - Release
> Date: 07/01/2007 18:29
>
>
--
No virus found in this outgoing message.
Checked by AVG Free Edition.
Version: 7.5.432 / Virus Database: 268.16.7/619 - Release Date: 07/01/2007
18:29
More information about the TheForge
mailing list