   I guess I will just stick to the sheet metal and smaller pieces. Work
   up some experience before I tackle any larger stainless projects. I
   still might hide that piece of 2" shaft away for some later date.

Harry


On Tue, 2 Jan 2007 13:24:27 -0800, "Grant Marcoux"
<gblacksmith at alamedanet.net> said:
> Though highly forgeable, stainless steels are typically far harder to
> forge
> without cracking.  They usually have poor heat retention and transfer
> characteristics due to the typically high amounts of chromium and other
> refractory elements present.
> 
> Most non-martensitic stainless steels that are not heat treated can be
> cut
> on a horizontal band saw without too much protest.  When in doubt, check
> it
> with the edge of a file and a hacksaw.
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net]On Behalf Of Harry
> Sent: Tuesday, January 02, 2007 9:18 AM
> To: Sponsored by ABANA
> Subject: [TheForge] Stainless steel tools
> 
> 
> Hi all,
> 
>     If I am to work with stainless should I make hardies and such out of
>     stainless as well? And on the subject of stainless does it forge
>     well? I haven't tried any yet but they produce a lot of stainless
>     scrap at work. I was looking at a 2" shaft they were throwing away
>     and thinking it could be used for a lot of things...if it can be
>     forged. I don't have a plasma cutter so it would have to be cut the
>     old fashioned way. What I have been working with so far would be
>     A36, leaf springs, any bits of steel that were handy. I have some
>     fairly large gauge copper wire I have been playing with as well.
> 
> Glad the holidays are over.
> Harry, aka Ebeneezer
> --
>   Harry
>   iowaharry at fastmail.net
> 
> --
> http://www.fastmail.fm - IMAP accessible web-mail
> 
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 
> 
> 
> --
> No virus found in this incoming message.
> Checked by AVG Free Edition.
> Version: 7.1.409 / Virus Database: 268.16.1/611 - Release Date:
> 12/31/2006
> 
> 
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 
-- 
  Harry
  iowaharry at fastmail.net

-- 
http://www.fastmail.fm - Access your email from home and the web



More information about the TheForge mailing list