I suspect his weight listing is 0 3 21, which would be 105 lbs.
Or maybe it's (blank) 3 21. Someone may have been sloppy with the number punches.
Rob
---- kim george <klgeorge at kent.edu> wrote:
> The numbers on the side of the pw anvil the 3 means 3 english hundred
> weight (110 lbs.?) the 2 is 1/4 hundred weights and the 1 are single
> pounds. If the hard table is in good shape (no major chips,cracks, and
> there is no buzz when you tap it [means broken weld between hard face and
> base] ). It is hard to find a P.W. that size. If your not going to try to
> lug it around to do shows or demos that anvil will do you good service for
> your lifetime and the next smith's. I wouldn't pass it up.
>
> Kim George
>
> "Why for you burry me in cold,cold ground?" Taz
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
More information about the TheForge
mailing list