Does your burner(s) have a means to adjust the combustion air going into the
burner? If not, you will not be able to restrict the amount of air to get
close to stiochometric point and this usually means excess air and lots of
scaling/oxidation. A little excess air generally raises the temp but too
much drives the temp down.
I also use Larry's side arm style and have to throttle the air down quite a
bit. I don't have any instrumentation so I adjust so flames have slight red
edges and open a bit more. Helps to do in a darkened shop.
Rick Korinek
Island City Forge
Minocqua, WI
islandcityforge.com
715/358-5060 shop/studio
715-892-7425 cell
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Steve Smith
Sent: Tuesday, February 13, 2007 6:05 AM
To: Sponsored by ABANA; frosty at customcpu.com
Subject: [TheForge] Sidearm burners
Jerry Frost wrote:
> A jet ejector type burner like the: Fisher, Porter, Rex's series,
> sidearm, "T" jet, etc. have the air intakes at 90* to the jet. A
> commercially designed jet ejector will induce a max of 29:1. (gas to gas)
>
> Don't ask me why simply moving the air intakes makes so much difference
> to the induction rate, I don't have any idea. What it means for us is a
> more efficient and easier to make burner. If you build a linear you have
> to hit it pretty darned accurately to get a 16:1 ratio for a neutral
> burn. If you build a jet ejector you have a LOT of tolerance to play
> with. I like easy. <grin> This is why such crude designs as the "T" jet
> and Sidearm work so well, there's just a lot of room to play with.
I'm responding to Frosty's comments, but welcome replies from all.
I'm still messing with burners in a very slow fashion. I've made maybe a
dozen Reil burners and have been very happy with their performance. I
make the jet out of 1/8" brass pipe, aligned with the axis of the
burner, jet hole drilled in the brass end cap.
I was pretty interested in sidearm burners when they were first
discussed. I followed in Frosty's footsteps and experimented with a 4
way pipe fitting instead of a sidearm. It was ok, but not as good as the
Reil burners, which I chalked up to not having a smooth transition to
the 3/4" body.
Then I saw that Larry Zoeller had added a sidearm 'kit' (all you have to
do is tighten things up). I bought one of these. It came with a tapered
mig tip for the gas jet, pretty nice setup and for not much more than
the fittings would have cost me. I recently compared the performance of
this sidearm burner to a Reil burner. Both are 3/4" body with Larry's
stainless flares on the end. I measured with a thermocouple, both in the
same, single burner forge.
The sidearm was almost as good as the Reil burner. Final temp was maybe
100 degrees lower. This makes me think that the sidearm is just an easy
way to put the same burner together, and less impressed with the mig
tip. Sounds like this isn't correct--what am I doing wrong?
I'm at maybe 300' above sea level, neither burner has a choke. Pictures
could be done if important to the plot.
Thanks,
Steve
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list