I don't recall who it happened to but someone (I think)
on this list made a chip bed forge using one of Mikey's
burner designs and melted the 3,000f kiln shelf he was
using for the fire grate.
Frosty
-------------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks
Meadow Lakes, AK.
http://www.artmetalradio.com/
From: "Jerry Smith"
<jerry_smith at anvilsandinkstudios.com>
> Jim,
>
> I would very happy if the burners for my foundry
> setup
> would burn at 2,400 degrees F. I have a NC Tool
> Whisper Daddy, and it gets plenty hot, above 2,200
> degrees F.
>
> So far I have seen complex burners and not so complex
> burners, they all have the same basic structure. I
> like Frosty's deaign, because it is really simple and
> hard to mess up.
>
> Jerry
>
>