I was thinking jewelry type of damascus for this
stuff.

So I will strap a bunch of it together to make bilets
from.

Thanks,

Jerry
--- "Mark A. Pesetsky" <pesetsky at Princeton.EDU> wrote:

> Jerry,
> 
> I have a whole roll of this material and my test of
> the material proved
> it to be mild good for furniture or trinket
> damascus...
> 
> Mark 
> 
> 
> I have a bucket full of banding steel, would this be
> good for making
> bilets or some kind of pratice damascus?
> If it is just junk steel, it will go to teh
> recycling pile.
> 
> Merry Christmas,
> 
> Jerry
> 
> 
> 
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 
> 



More information about the TheForge mailing list