[TheForge] Wrought iron

Albin Drzewianowski dski1045 at qis.net
Tue Aug 28 16:48:30 EDT 2007


Mark,

Do you have access to a power hammer??

There is a guy from somewhere in the midwest that has a large amount of 
wrought iron from a fence that was taken down.  He is selling 1" square rod. 
He has advertised in the classified section of ABANA's "Anvil's Ring".

I bought some from him at Gichner's this past January and it seems to be 
pretty nice stuff.  Forge welds nicely.   He had quite a bit.    As far as I 
know he only has square rod.

Do you still get the "Anvil's Ring"  if not, I will hunt up a copy and get 
you the contact info if you are interested.

Regards,
Albin
Westminster, MD

----- Original Message ----- 
From: <williamsiron at comcast.net>
To: <theforge at mailman.qth.net>
Sent: Tuesday, August 28, 2007 4:17 PM
Subject: [TheForge] Wrought iron


I have a customer that would like some strap hinges made of wrought iron. 
The hinges will be approximately 27" long by 3" wide at the barrel. The 
question is: Where is there a source to buy good wrought iron? I know of one 
in England but none in the States. Any help is appreciated.

Mark
Snow Hill, Maryland
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________





More information about the TheForge mailing list