Mark,
Yeap that one, it has worked for two years now. It
goes on sale for about $160 every so often. I have
done silver, gold, brass, copper, platinum, tin and
other soft metal in it. I was not meant for steel, so
I don't do that metal in the mill.
Jerry
--- "Mark A. Pesetsky" <pesetsky at Princeton.EDU> wrote:
> This one:
>
>
http://www.harborfreight.com/cpi/ctaf/displayitem.taf?Itemnumber=4832
>
> Mark
>
>
>
> I have the one that HF sells, it works great, plus
> if you can turn steel
> (S7) you can make your own rollers.
> In the trade they are called Rolling Mills.
> Jerry
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list