Thank you for your response Mike. An additional question, if I may.
Once the roaster is used by the end-user, perhaps even once over a
campfire or bbq, would I assume the wax would melt off? Even after
its use and washing by hand, won't the beeswax wear off and have to
be re-applied for fear of rusting? Beeswax to keep on-hand for the
average end-use consumer, may be difficult to find. This may be a
good solution to get the item initially out the door, but perhaps not
a returning customer.
---
On 11-Oct-06, at 7:25 PM, Mike Linn wrote:
> I use bees wax.
>
> heat until wax smokes and spread all over. Buff with a cotton cloth
> and it looks great.
>
>
> mike
>
>
> At 01:07 PM 10/11/2006, you wrote:
>> Speaking of finishes...
>> What about finishes for items that will come in contact with food,
>> like wiener roasting forks, roasting pokers, etc.?
>> ---
>> Marsha
>> Blenheim, Ontario
>>
>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> password: anvil
>> ___________
>>
>
>
> Mike Linn
> Artist Blacksmith
> McCalla, AL
> AFC Webmaster
> http://afc.abana-chapter.com
>
> ______________________________________________________________________
>
> "Many of life's failures are people who did not realize how
> close they were to success when they gave up. "
> ~ Thomas A. Edison
> ______________________________________________________________________
>
>
>
>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
More information about the TheForge
mailing list