[TheForge] Lawn Mower Blade

Bob Ehrenberger eforge at centurytel.net
Wed Oct 4 09:33:24 EDT 2006


Jerry,

I have a friend that is into Gravely equipment and it's my inpression that
there is a lot of support out there, both new and used parts.  You shouldn't
have a problem finding replacement blades.

Are the blades on your Gravely missing or just worn out?

Robert Ehrenberger
Shelbyville, Mo.
eforge at centurytel.net

------Original Message-----
From: Jerry Smith <jerry_smith at anvilsandinkstudios.com>
Subject: [TheForge] Lawn Mower Blade

I will be picking up an older Gravely lawn mower
tomorrow. We have been looking for a mower for our
grassy lawn acreage and found one.

What I was wondering is, can I forge a blade for this
mower? I can drill and machine such things, but I
think this has a curl to the cutting edge, can I
hammer this out with the heat and beat process?




More information about the TheForge mailing list