[TheForge] Iron-Iron Carbide Phase Diagram Example

dann at wctatel.net dann at wctatel.net
Mon Oct 2 07:46:09 EDT 2006


Note that the little black dots inside of the wikipedia graph are
-CLickable -  for more detailed explanation.

Dann

> Here's a great diagram I found via Wikipedia:
>
> http://www.sv.vt.edu/classes/MSE2094_NoteBook/96ClassProj/examples/kimcon.html
>
> Bruce