Did they perform repeated blows or were they just trying to strike hard enough to chip or crack one?

I would assert that repeated blows is the key.

Ray
Cincinnati

---- Justin Fisher <justinf at pixelations.com> wrote: 
> Mostly they were using claw hammers, set up in a rig to smack two 
> hammers face-to-face.  They even tried hardening the hammers, and at the 
> end they aimed a hammer at Chinese Anvil-Shaped Object.  No shattering, 
> not even any chipping.
> 
> They concluded that hammers don't shatter, even if abused.
> 
> Comments?
> 
> 
> --Justin Fisher,
> generally avoiding hitting my hammers with other hammers.
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 



More information about the TheForge mailing list