In this liability suit plagued nation, prudent mfgs don't go for
maximum hardness for struck faces any more, i'd guess.
But i've had hammer faces chip and spall when they whacked a
hardened surface.
Striking the face of an ASO is simply an exercise in despair.,,,pf
Justin Fisher wrote:
> Mostly they were using claw hammers, set up in a rig to smack two
> hammers face-to-face. They even tried hardening the hammers, and at the
> end they aimed a hammer at Chinese Anvil-Shaped Object. No shattering,
> not even any chipping.
>
> They concluded that hammers don't shatter, even if abused.
>
> Comments?
>
>
> --Justin Fisher,
> generally avoiding hitting my hammers with other hammers.
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list