Jim,
Thanks! That's what I thought. She go the idea from the "Old French Country" look.

Ray 
---- James Binnion <jbin at well.com> wrote: 
> Ray,
> 
>   Solid zinc sheet is / was used  to make countertops and sinks just  
> like copper. It was soldered with tin/lead or tin/zinc solder. I  
> would suggest the tin/zinc for food areas :-)  Make sure to bid in  
> some learning costs as it is not a trivial undertaking it is much  
> tougher to work than copper.
> 
> Jim
> 