Garden Gates by Gary Meyer wrote:

> Yes you are correct.  acetylene FIRST.

The O2  should be turned off first or the possibility of  flash back may 
occur.
Although with flash suppressors standard now I guess this is not a problem.
 
 A one way valve attachment is the deal I am trying to attach a word to.
The flash suppressor is what was on the barrel of my M-16.

Kenny O