[TheForge] Re: Harbor Frieght
Jerry Frost
frosty at customcpu.com
Tue Nov 21 21:14:59 EST 2006
I have a horizontal/vertical bandsaw I got from a tool
closeout place some 20 years ago. It's gotten worn
enough I have trouble keeping it tracking, even with
new bearings. It's a dry saw and as you say, with
bimetal varitooth blades it worked just fine, (while
it'd track that is)
I bought a 7" x 12" Jet horizontal/vertical wet bandsaw
and using bimetal varitooth blades it works just fine
as well. The trick if you're going to use it dry is to
slow it down a step on the pullys and using the right
tpi for the stock thickness is more important.
A wet saw is good for dirty or old stock as it washes
the grit so the blades don't dull as fast. Of course
taking a wire brush to dirty stock makes for longer
blade life in either case.
Frosty
-------------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks
Meadow Lakes, AK.
http://www.artmetalradio.com/
From: "Darrell" <darrell67 at machinemaster.com>
>I had been thinking of getting or making a lube system
>for my saw but then I found that good bi-metal vari
>tooth blades to be a much cleaner and in the long run
>cheaper solution.
>
> Darrell
>
>
>
More information about the TheForge