[TheForge] ranite hardfacing rods
Dan Tull
dantull at numail.org
Wed May 24 17:53:25 EDT 2006
Or if you really don't care any more than that , use JB weld.
----- Original Message -----
From: "Washington, Aubrey O." <awashington at ou.edu>
To: <munlaw2 at hcsmail.com>; "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Wednesday, May 24, 2006 4:37 PM
Subject: RE: [TheForge] ranite hardfacing rods
I'll try it! Thanks for the suggestion.
________________________________
From: theforge-bounces at mailman.qth.net on behalf of Ron Childers
Sent: Wed 5/24/2006 3:14 PM
To: 'Sponsored by ABANA'
Subject: RE: [TheForge] ranite hardfacing rods
You may have to can it with a refractory to concentrate the heat but it
should do it
--------------------------------------------------------------------------------
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list