[TheForge] ranite hardfacing rods

Peter Fels And Phoebe Palmer artgawk at thegrid.net
Tue May 23 22:45:36 EDT 2006


Respectfully Ron;
I don't thing 7018 is at all adaquate for use on an anvil 
face..Pete F

Ron Childers wrote:
> I think u would have ur hand too close to the preheated anvil to use tig. If
> 
> U want to remove gashes just preheat to 350 and stick weld with 7018 and
> pien it while it cools.
> 
> 
> 
> 
>  
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of schade at acegroup.cc
> Sent: Tuesday, May 23, 2006 12:13 PM
> To: Sponsored by ABANA
> Subject: Re: [TheForge] ranite hardfacing rods
> 
> 
> On May 23, 2006, at 10:44 AM, Luke Thomson wrote:
> 
> 
>>After reading your reviews I am doubting that my anvil needs to be 
>>refaced, just repaired. I plan on getting some sticks or maybe wire if 
>>I can today. I've posted some pictures on photoaccess under tools and 
>>tooling ( it wouldn't let me create a new album...)  My pictures show 
>>the gashes but I was unable to show the sway very well.
> 
> 
> 
> Does anyone know any reason why not to run tig beads across the anvil? 
> 
>>Seems like that would both reduce the amount of grinding and, more 
>>importantly, give me some more practice with TIG.
> 
> 
> 
> 
>>Thanks for all your help,
>>Luke
>>
> 
> 
> 
> 
> couldn't find your pictures. Some sway isn't really that big a problem. 
> My advice would be to get something you can use as an anvil. track, 
> large object etc. After working a while you will know better what your 
> requirements are. don't get bogged down in having a perfect anvil.
> 
> Bob
> 
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 
> 
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 
> 
> 


More information about the TheForge mailing list