> Roger,
>
> Jeff @ mockingbird Forge bought a Turkish hammer @ the
> 2001 Madison conference. We have used it hard every day
> with very few problems; a few minor adjustments and a
> start capacitor on the motor. We wore out a couple sets of
> dies but as Uri would say, "Is good tool". It is very
> ergonomic and user friendly. I don't know where you live,
> but you are welcome to use the big mean green machine if
> you haven't used one. That way you can see what it will do
> and find out if it likes you.
>
>
> Also, several friends have Big Blues and are happy with
> them plus they cost a lot less and they will finance. You
> do have to have a separate air compressor but there are
A shop I know that went defunct and has a Bull hammer has
to use a huge air reservoir in order to run with out an
issue even with the compressor they have which is a large
American kellog that has a 7HP Bador motor.
By the way I would jump all over this but it is too large
of a setup for my shop. If any one is in need of any of
these items I know the owners and I am sure they will
acept any reasonable offer. It would be pickup only in WA
state by Seattle. Rereading that I guess that came off as
a shameless plug. Sorry.
Martin
> dozens of other uses for a high cap compressor. I have
> used and like both; they do what they are supposed to do
> but I don't have any info on the cost of electricity to
> run each. Ask Dan about his. It has performed faithfully
> for years. Try several and note your likes and dislikes on
> each. A new power hammer is like getting married. It is a
> big investment and it's best to be sure before you commit
> yourself.
>
> Ron Childers
>
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of
> Roger R Degner Sent: Wednesday, May 10, 2006 5:52 PM
> To: 'Sponsored by ABANA'
> Subject: [TheForge] Air hammer recommendations?
>
> I was at BAM conference and am considering buying one of
> Tom Clark's air hammers
> Anyone have feed back good or bad about this hammer. I
> believe they are imported from Turkey.
>
> Roger R Degner
>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
More information about the TheForge
mailing list