[TheForge] Drawing Down Bar Stock

debmiller at fuse.net debmiller at fuse.net
Mon May 8 12:31:04 EDT 2006


Hi People!

After all these years I come to realize I have never drawn rectangular bar stock. Round, square, but not rectangular.

I don't want to wast a bunch of material on trial and error for an urgent project.

The bar stock is 1/2" x 2". 

Hints?


Ray
Cincinnati