> In the front axle of the old VW bugs are a bunch of flat springs, torsion
> springs, I think.
That's right.
> Does anyone know what kind of spring steel was used?
Not by spec, but it's air-hardening. Heat it, let it cool in air,
file glides off. I think I have one narrow piece here somewhere.