[TheForge] FW: ITC 213 question

Ralph Sproul brhlbsmt at mcttelecom.com
Wed Mar 29 07:31:52 EST 2006


	Martin, for what it's worth - I used ITC 100 years ago that was a beige in
the jar color - ended up white after firing.

	Have not used the ITC 213......no info there.

Ralph

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net]On Behalf Of Martin Paietta
Sent: Tuesday, March 28, 2006 11:10 PM
To: 'Sponsored by ABANA'
Subject: RE: [TheForge] FW: ITC 213 question


Anyone have any thoughts on this?

Thanks
Martin

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Martin Paietta
Sent: Sunday, March 26, 2006 8:21 PM
To: theforge at mailman.qth.net
Subject: [TheForge] FW: ITC 213 question

I just recieved a bottle of ITC 213, is it supose to be brown or does it
turn more of a white or gray after firing. I was redoing the ceramic coating
in my forge and it was recommended to me to put a top coat of ITC213 (I know
213 is for metal). When would you put the top coat on? After the base coat
drys, after one fireing, or after all of the firings?

Thanks
Martin
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________

_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________






More information about the TheForge mailing list