I posted a photo of the three sizes I picked up in the "Forges" section of the
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil

At 09:27 PM 3/3/2006, you wrote:
>So here is the info laguna clay
>GRINDING BALLS
>These high quality white alumina grinding balls are non-contaminated and
>assure
>thorough mixing and grinding.
>Approx. Balls
>Per # 1 lb. 5 lbs. 10 lbs.
>TM-309 1/2" 100 $4.90 $4.40 $3.95
>TM-310 3/4" 35 4.45 4.00 3.55
>TM-311 1" 16 4.00 3.60 3.20
>TM-31114 11/4" 8 4.25 3.85 3.40
>Prices are per pound. Typically jar is filled 55% with grinding balls.
>
>Ceramic Supplies & Solutions Since 1932 130 (800) 4-LAGUNA . (626) 330-0631
>. info at lagunaclay.com . www.lagunaclay.com
>Dan in Auburn

Michael D. Horgan , lughaid at earthlink.net
http://members.aol.com/lughaid/
posting from
  A BRAZEN FORGERY
Blacksmithing and Metalwork
Claremont, Ca.




More information about the TheForge mailing list