[TheForge] Mosquito control in quench bucket?

Rick rick at smokyforge.com
Thu Jun 29 07:52:53 EDT 2006


They are called Mosquito Dunks  and are available locally at the Farm and 
Fleet Store.  My wife says they should also be at garden stores.

Rick


----- Original Message ----- 
From: "Rick" <rick at smokyforge.com>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Wednesday, June 28, 2006 4:05 PM
Subject: Re: [TheForge] Mosquito control in quench bucket?


>I use those donut shaped tablets that are made to keep out mosquitos.  Oil 
>could get soaked up into the wood and keep it from soaking up water any 
>more, thereby causing leaks.  Anyhow, that is my thought.
> When my wife gets home, Ill ask her what the right name of these tablets 
> is.
>
> Rick Crawford at Rafter Lazy C
>  Home of Smoky Forge and Lem the Wonder Mule
>   In the middle of Northern Illinois
>
>    http://www.smokyforge.com
>     rick at smokyforge.com
>
>
> ----- Original Message ----- 
> From: "Mitch Widham" <widha8d3 at erau.edu>
> To: <theforge at mailman.qth.net>
> Sent: Wednesday, June 28, 2006 9:01 AM
> Subject: [TheForge] Mosquito control in quench bucket?
>
>
>> Help.
>>
>>
>>
>> I am just starting out as a hobbyist blacksmith, and received a nice old
>> half oak barrel for father's day. What is the best way to keep out the
>> mosquitos? I don't think a cover will work because the top is uneven. I 
>> am
>> looking for something that is cheap, easy, effective and won't negatively
>> affect the quench? Am I asking too much?
>>
>>
>>
>> Mitch Widham
>> Operations Supervisor
>> Campus Safety Department
>> v: 7580
>> f: 4932
>> mitchell.widham at erau.edu
>>
>>
>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login:  blacksmithblacksmith at hotmail.com
>> password:  anvil
>> ___________
>>
>>
>>
>>
>>
>> -- 
>> No virus found in this incoming message.
>> Checked by AVG Free Edition.
>> Version: 7.1.394 / Virus Database: 268.9.4/375 - Release Date: 6/25/2006
>>
>>
> 



-- 
No virus found in this outgoing message.
Checked by AVG Free Edition.
Version: 7.1.394 / Virus Database: 268.9.6/378 - Release Date: 6/28/2006



More information about the TheForge mailing list