On Jun 17, 2006, at 6:31 PM, Mike Porter wrote: > Jeff, > Historically speaking then: the design is Victorian era, when > casting was > king. > Mikey > Yes but cast iron is useless for this kind of thing. Cast steel was not really happening at that time. Those items were forged chiseled and filed to shape. James Binnion jbin at well.com