From: "James Binnion" <jbin at well.com>
> This thing about buss bar w berylium comes up every
> so often. Beryllium copper looks more like brass or
> bronze it is distinctly yellow cast to it. Second
> almost all buss bar is C101 or C102 (oxygen free
> copper) because this has the lowest IxR losses. The
> only time beryllium copper is used is when the
> strength that it provides is needed as it is quite a
> bit more expensive than most copper alloys.
>
> For forging use C101, C102, C110 they are all easy to
> work hot or cold
>
> Jim
>
>
>
> James Binnion
> jbin at well.com
>
>