[TheForge] Forging copper
dave mudge
dave at magichammer.net
Sun Jun 18 00:42:19 EDT 2006
Don,
I think that ground rod is copper coated steel rod.
Bus Bar from old electrical service boxes can be 1/4" x 2"
I have forged some of that. Check your local scrap yard
or electrical supply house.
dave m
NOTICE: Due to Presidential Executive Orders, the National Security Agency
may have read this email without warning, warrant, or notice.
They may do this without any judicial or legislative oversight. You have no
recourse nor protection.
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net]On Behalf Of PlumDon at aol.com
Sent: Saturday, June 17, 2006 7:41 AM
To: theforge at mailman.qth.net
Subject: [TheForge] Forging copper
Can anyone recommend an easy forging copper in rod or bar? What about
grounding rod or is it too red short? Need something large enough to forge a
dozen
or so drawer pulls.
Kindest thanks for any suggestions
Don Plummer
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
--
No virus found in this incoming message.
Checked by AVG Free Edition.
Version: 7.1.394 / Virus Database: 268.9.0/368 - Release Date: 6/16/2006
--
No virus found in this outgoing message.
Checked by AVG Free Edition.
Version: 7.1.394 / Virus Database: 268.9.0/368 - Release Date: 6/16/2006
More information about the TheForge
mailing list