From: "Bill Roberts" <robertsb at pig.net>
> there are a variety of ways.....but a good low tech
> approach is to fire up your Ox/acet
> torch............Just the acet. and soot up the
> piece of aluminum.
> bill
> On Jun 12, 2006, at 9:16 AM, robert hensarling wrote:
>
>> What would be considered a proper annealing temp for
>> aluminum and copper?
>
> Bill Roberts
> www.CustomDesignMetalArts.com
>
You can also use a Sharpie marker to indicate temp for
AL. Mark and heat till it disappears. There will be a
faint mark left so don't keep heating till it's gone
completely!