Chris Kilpatrick wrote: > hi Folks, > I have been having a little trouble forge welding recently. I found a pool of nickel in my forge (from quarter mokume), could that be interfering with my welds? I found some of the nickel had adhered to my billet. > Yeah, stuff like that contaminates the forge. Is it a gas forge? Coal?