[TheForge] Bronze
roger olsen
erik at methow.com
Thu Jun 8 13:22:03 EDT 2006
> For that, I use Naval Bronze, which is C465- It has a bit of lead in it,
> and some zinc, both of which make it trickier to forge, and much tougher
> to weld. But the forgeablity is good, and the color is beautiful.
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
Hi Ries,
Do you know of any dangers that may be associated with forging Naval Bronze
because of the lead or the zinc?
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
----- Original Message -----
From: "Ries Niemi" <rniemi at fidalgo.net>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Thursday, June 08, 2006 10:16 AM
Subject: Re: [TheForge] Bronze
> Everdure is a trade name for Silicon Bronze, which is C655.
> Its mostly Copper, with a tiny bit of silicon in it.
> I think its the best bronze to start with- it forges nicely, can be tig
> welded, and is available in a variety of sizes and shapes.
>
> Here are some places to get it:
> http://www.alaskancopper.com/
> http://www.copperandbrass.com/public/division/project/html/home.html
> http://www.atlasmetal.com/
> http://www.farmers-copper.com/
>
> Learning to get it hot enough, but not too hot, is the hardest thing to
> learn- too cold, you get cracking.
> But too hot, and all of a sudden, you got nothing but a puddle.
> I tend to turn the lights down, and look for the slightest red glow, in
> the dark. Not a bright enough red to be even visible in sunlight.
> In normal shop light, I will forge it in the purple and browns- well below
> when it starts to get dull red in full light.
>
> Its fun to forge, moves pretty easily.
> The biggest drawback to Silicon Bronze is the dark brownish red color when
> cold- it doesnt have that Yellowy, "Bronze" color.
> For that, I use Naval Bronze, which is C465- It has a bit of lead in it,
> and some zinc, both of which make it trickier to forge, and much tougher
> to weld. But the forgeablity is good, and the color is beautiful.
>
> Be forewarned- none of this stuff is cheap- copper has gone up a lot this
> year, and in addition to the per pound price of the base alloys, you get
> charged more for certain profiles- round bar is bad enough, but try
> pricing square bar or flat bar or angle, if you want to really punish
> yourself.
>
> ries
>
>
>
>
>
> On Jun 8, 2006, at 10:03 AM, roger olsen wrote:
>
>>
>>
>>
>>> everdure is considered the best bronze for forging and I would think if
>>> you
>>> googled 'forging everdure' you would get some good feedback. Actually
>>> I am
>>> not positive everdure has an E on the end but I think so.
>>>
>>> Anvilfire may also have some instructions about forging bronze.
>>>
>>> I have forged it and the smaller the stock the more frustrating. I did
>>> not
>>> find it as easy to forge as copper but it is definitely doable. You
>>> will
>>> need to experiment but the learning curve will start out very steep.
>>> You do
>>> not want to bring it up where it shows color, just below that as I
>>> recall,
>>> keep your forge turned low, too hot or too cold and it will break like
>>> a
>>> stale oatmeal cookie. Try rubbing the stock with a block of wood at
>>> different temp and note when it feels greasy and note the type and
>>> quantity
>>> of smoke it creates and try forging. The hardest part is finding the
>>> 'window' of not to hot, not to cold.
>>>
>>> Good luck
>>>
>>> Roger Olsen
>>> ~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
>>> ----- Original Message ----- From: "robert hensarling"
>>> <rhrocker at hilconet.com>
>>> To: "Sponsored by ABANA" <theforge at mailman.qth.net>
>>> Sent: Thursday, June 08, 2006 9:49 AM
>>> Subject: [TheForge] Bronze
>>>
>>>
>>>> I'm wanting to try my hand at forging a little bronze. I'm going to
>>>> buy
>>>> just a little (one sq. foot) of 1/16th" and also some bronze rod for
>>>> vines,
>>>> probably just 3/8's".
>>>>
>>>> Could anyone please tell me the class (220, etc) for the sheet and rod?
>>>> This is my first venture and would like to get the numbers right. I
>>>> already
>>>> have Silicon Bronze rods for my tig (don't know if it can be forge
>>>> welded,
>>>> but if it can, I'm more than positive that I couldn't do it very well).
>>>>
>>>> Seems that someone once said to use a outfit in Denver for the stuff,
>>>> Atlas
>>>> Metal I think.
>>>>
>>>>
>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> password: anvil
>> ___________
>>
>>
>>
> Ries Niemi
> Industrial Artist
>
> http://www.RiesNiemi.com
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
More information about the TheForge
mailing list