The copper I use must be heavier than his. I found that if I didn't 
anneal, it work hardens and tears.
Chris

Steve Smith wrote:

> You got it in one Chris. I think he said he adds talc to it to make it 
> stiffer. He said he doesn't anneal much, he might have to once each 
> piece or not at all.
>
> Steve
>
> Chris Worsley wrote:
>
>> Jeff,
>> It looks like he uses plasticene, an oil based modeling clay. The 
>> kind I think he uses is white, and there are some small pieces on the 
>> table in some of the pictures that have been posted.
>> One of the students (Frank) on his website has some on his table too.
>> Using plasticene or plastilene lets you work a lot quicker because 
>> you don't have to deal with the heating of pitch and the cleaning off 
>> of the piece each time you switch to the other side.
>> When you use something other than pitch, annealing more often is very 
>> important. I have found that you have to have the copper as soft as 
>> possible for as long as possible when using the clay. It (clay) does 
>> not get as hard as the pitch and offers less resistance to the 
>> tools.  I was amazed by the detail he gets with clay. I switch to 
>> pitch for that kind of tiny detail at the end of the process.
>>
>> Chris
>> AZ
>>
>> Jeffrey Polaski wrote:
>>
>>> Wow. That's some incredible stuff.
>>> It says he doesn't use pitch. I wonder if he uses anything for a 
>>> backing
>>> material. On the "How It's Done" page the work looks like it elevated,
>>> with a block of something under it. Does anyone know what that block 
>>> is?
>>>
>>>
>>> Anyone have more on how he does it?
>>> Jeff Polaski
>>> Research and Graduate Studies Webmaster
>>> University of California, Irvine
>>> http://www.rgs.uci.edu/
>>> 949.824.6363
>>>
>>> -----Original Message-----
>>> From: theforge-bounces at mailman.qth.net
>>> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Steve Smith
>>> Sent: Thursday, July 13, 2006 7:33 PM
>>> To: Sponsored by ABANA
>>> Subject: Re: [TheForge] ABANA conference
>>>
>>> I was really impressed with Dadyan's work. He teaches classes too.
>>> http://www.melicdadayanart.com/index2.html
>>>
>>> Steve
>>>
>>> Chris Worsley wrote:
>>>
>>>  
>>>
>>>> Thanks! Good shooting.
>>>> Especially liked the series on repousse.
>>>>
>>>> Chris
>>>> AZ
>>>>
>>>> Steve Smith wrote:
>>>>
>>>>  
>>>>
>>>>> Ok, you asked for 'em, you got 'em.
>>>>>
>>>>> I put a selection of the photos I took on my web page. I shrank 
>>>>> all the photos and compressed the directory--it is now only 5Meg. 
>>>>> You'll really wish you had broadband if you don't:
>>>>>
>>>>> http://users.frii.com/sos/Steve/
>>>>> The file name is AbanaAbridged.zip
>>>>>
>>>>> Steve
>>>>>     
>>>>
>>>>
>>>>
>>>>
>>>>
>>>> _______________________________________________
>>>> Manage membership or unsubscribe at:
>>>> http://mailman.qth.net/mailman/listinfo/theforge
>>>> theforge mail list group photo site is
>>>> http://www.photoaccess.com
>>>> Login:  blacksmithblacksmith at hotmail.com
>>>> password:  anvil
>>>> ___________
>>>>
>>>>
>>>>
>>>>   
>>>
>>>
>>> _______________________________________________
>>> Manage membership or unsubscribe at:
>>> http://mailman.qth.net/mailman/listinfo/theforge
>>> theforge mail list group photo site is
>>> http://www.photoaccess.com
>>> Login:  blacksmithblacksmith at hotmail.com
>>> password:  anvil
>>> ___________
>>>
>>>
>>>
>>> _______________________________________________
>>> Manage membership or unsubscribe at:
>>> http://mailman.qth.net/mailman/listinfo/theforge
>>> theforge mail list group photo site is
>>> http://www.photoaccess.com
>>> Login:  blacksmithblacksmith at hotmail.com
>>> password:  anvil
>>> ___________
>>>
>>>
>>>
>>>
>>>  
>>>
>>
>>
>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login:  blacksmithblacksmith at hotmail.com
>> password:  anvil
>> ___________
>>
>>
>>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
>
>





More information about the TheForge mailing list