This looks to be precision ground drill rod. MSC sells decarb free 
rounds (not precision) for *far* less money:
http://www1.mscdirect.com/CGI/N2DRVSH
$22 instead of $90, and MSC is a very good place to deal with. They will 
take credit cards, personal as opposed to company doesn't matter. 
Careful, they have lots of fun stuff.

If you want a larger quantity, I've bought several times from Crucible 
Steel. Their prices were a lot more reasonable than the specialty tool 
steel sellers I checked out. I don't know what their minimum is, but I 
remember at least one order that was about $75. You may have to dig a 
bit to find your local stocking point.

Steve

Gabriel Cain wrote:

> http://www.onlinemetals.com/merchant.cfm?id=184&step=2&showfrac=yes
> 
> Jeffrey Polaski wrote:
> 
>>I'd like to get some S-7 to make some few punches out of. I'm looking
>>for about 1/2" square, or a little larger round or hex stock. Anyone
>>have a good source?
>>
>>
>>
>>Jeff Polaski
>>Research and Graduate Studies Webmaster
>>University of California, Irvine
>>http://www.rgs.uci.edu/
>>949.824.6363
>>
>>
>>_______________________________________________
>>Manage membership or unsubscribe at:
>>http://mailman.qth.net/mailman/listinfo/theforge
>>theforge mail list group photo site is
>>http://www.photoaccess.com
>>Login:  blacksmithblacksmith at hotmail.com
>>password:  anvil
>>___________
>>
>>
> 
> 
> 


More information about the TheForge mailing list