When working with long pieces I hang small rings from the ceiling
with small ropes at the appropriate height ( anvil or forge or power hammer
) to support the other end. Then all I have to do is manipulate the work
over the anvil or in the forge as needed. I made an S-hoop from a 20 foot
piece of 1/2 sq doing this - bending the piece was much more difficult than
forming the ends. The other option is several adjustable stands set ad the
right height.
Bob Willman
Bowling Green, Ohio
The Eagle's Anvil
WB8NQW
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Rick Korinek
Sent: Tuesday, January 24, 2006 11:19 PM
To: 'Sponsored by ABANA'
Subject: [TheForge] 2 Questions
Hello all. I have two questions that relate to jobs coming up.
First, what kind of finish do you use for fireplace doors? What do you use
vs. paint that will stand up to the high temps encountered--especially when
using mild steel? In the case at hand, the client is interested in screen
doors out of bronze with bronze screen. I would like to patina down from
shinny then protect/coat to fix or slow further darkening.
The second question has to do with material handling. There are numerous
situations where one needs 10 to 16 feet of stock textured and/or worked--a
handrail for straight stairs, for example. I am at a loss for how to heat,
work in the power hammer and then straighten a long piece except to work
with smaller pieces and weld them together. I have worked pieces up to 7-8
feet long. This seems like the limit without a better system to support
work around the hammer and forge.
Very interested in your thoughts,
-Rick
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list