Stephen, If quenching the header and nail in water does not release the
nail, re-punch it to the way you think it ought to be and give it a whirl.
As with anything - even new doesn't mean it works right.
Ralph
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net]On Behalf Of
Steven.Walker at its.state.ms.us
Sent: Friday, January 20, 2006 9:50 PM
To: theforge at mailman.qth.net
Subject: [TheForge] nail header question
I recently purchased a nail header from Tom Clark at Ozark School of
Blacksmithing and I am having some trouble with nails getting wedged
in it after forming the nail head. I did some reading about nail
headers and how to make them and the tapered square hole in mine seems
to be punched in the opposite direction than what I've read you are
supposed to do.
The one I bought from Ozark S of B has the tapered hole larger on the
top of the dome and smaller on the bottom....like this:
======\ /
This originally seemed correct to me because that's the same direction
the nail tapers. However, hammering down on the head is pushing the
tapered nail into the tapered hole and making contact evenly on all
sides....and getting stuck.
However, after reading various blacksmith's instructions on how to
make one, they all seem to say to make the taper smaller on top of
the dome and larger at the bottom to keep the nail from getting
stuck.....like this: ======/ \
Seems with the hole tapered like the one I bought \ / , the nail gets
wedged and stuck when I form the head of the nail. I have to pound on
it to get it out and it always screws the nail up.
My question is what is the correct way to taper the hole in the nail
header. I wondering if Ozark S of B might have punched the taper in my
backward accidentally. Being a blacksmithing newbie, I'd like to here
some thoughts on this before I call and talk to Ozark S of B about the
nail header I bought. For all I know there are different schools of
thought on how to taper the hole.
You input will be greatly appreciated.
Thanks!
Steven Walker
Crystal Springs, MS
Confidentiality Note: The information containe= in this email and/or
document(s) attached is for the exclusive use of the=ndividual named
above and may contain confidential, privileged and no=-disclosable
information. If you are not the intended recipient, you =re hereby
notified that you are strictly prohibited from reading, phot
ocopying, distributing or otherwise using this e-mail or its contents
i=n any way. If you have received this transmission in error, please
noti=y me immediately.
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list