[TheForge] Sodium Bisulphate Pickle

Ralph Sproul brhlbsmt at mcttelecom.com
Fri Feb 24 06:58:57 EST 2006


"New Tidy Iron".......

I don't know if that would sell well.

Ralph

-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Todd Rich
Sent: Thursday, February 23, 2006 4:10 PM
To: Sponsored by ABANA
Subject: Re: [TheForge] Sodium Bisulphate Pickle



On Thu, 23 Feb 2006, Jonathan Nedbor wrote:

> Question for Bruce, or anyone else, what considerations are there for 
> clean-up/disposal of the sodium bisulfate solution when it is depleted.
>
> Jon Nedbor 
>
Well, considering sodium bisulfate is sold as toilet bowl cleaner.....
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________






More information about the TheForge mailing list